Quote:
Originally Posted by numbskull
It all went wrong.
Drying box too hot, maybe, caused pull away from the darter edges. New batch of epoxy, it skims in the cup and produces clumps when you brush it.
I want to build stuff for other people, but giving away this crap is embarrassing. It was all looking so good right up to that last step.
So it goes.
|
George, you might want to abandon the drying box and let them just spin for a day on your rod dryer as it seems to work best for me. My basement is about 70 degrees and the sys 3 sets up good in 12 hours and is real hard in 24. I can imagine the heated dryer will keep the stuff viscous longer than you want, thus the running problems may occur.
My stuff skimmed in the cup if I let it sit there too long and didn't stir it. If you treat the stuff like a cement mixer and keep stirring, the clumps are minimized.
Keep in mind here I'm doing small batches (30cc) and only coating 5-6 plugs at a time.
Finally, I hate to sound like a know it all on the sys 3 as I'm a rank beginner plug builder, but I've finished hundreds of fishing rods and the sys 3 properties are
much like aftcote properties with regard to mixing/applying, minus the clumping.