Quote:
Originally Posted by Tagger View Post
http://www.alumilite.com/ProdDetail....tegory=Casting Resins&Name=Alumilite White

good video .. no respirator ? .. Lets see $36.00 for 28 ounces = ? lures ... or $36.00 for 6) 6' 1.5 x 1.5 ayc = 36 lures min . wood is labor intensive and dusty ..
I used the regular not the white. The regular is stronger and has a shorter demold time. Also 6 bucks cheaper. I will get 25 usable needles from the 28 oz size. You also need to premeasure how much material you need to fill the mold or you will be throwing alot out either mixing too much or too little. I would like to make some swimmers but don't know if I really want to put the time and $ out to do it. I am real glad I tried it and it was fun and I learned alot but kinda takes the whole reason why I like doing this out of it. I like building whatever pops into my head and I get kind of uninterested in doing more than a few of any one thing. I had visions never having to turn another plug again. Lasted about 1 day.

Ted